Glass products are used in every aspect of our lives, but do you know? What is the most important part of glass products after production and processing? Yes, it is annealing. Today, let us further expand on the annealing process of glass in the furnace.
The annealing process of glass directly affects the quality and performance of glass. After the glass products are forced to be heated, deformed, cut or pulled during the processing, internal stress will be generated on the surface of the glass. This internal stress may cause the glass to shatter or even explode. The annealing process discussed today is the protagonist to solve this problem, that is, to weaken the internal stress on the surface of the glass through the annealing process to achieve the purpose of stabilizing the performance of glass products (we can use the annealing furnace to complete it). In addition, the annealing process can also effectively remove impurities and bubbles on the surface of the glass, thereby improving the transparency and appearance of the glass.
The process of glass annealing includes five stages: preheating stage, heating stage, slow cooling stage and cooling stage.
First of all, the preheating stage is the initial step of glass annealing. At this time, the glass can be slightly heated, but the temperature must not be too high, generally controlled at about 300°. This is because the heating temperature is very high in the later stage. In order to avoid the glass from being suddenly heated by high temperature and generating new internal stress, a preheating stage is designed to slowly adapt to the process from low temperature to high temperature. This is a very necessary step.
Then, in the heating stage, the glass products are heated to the annealing temperature to clear the internal stress. The annealing temperature is generally 20° to 30° lower than the upper limit of the annealing temperature, that is, the heating temperature is generally between 500° and 600°, and it is maintained for a period of time (the length of time is determined by the thickness, length and other parameters of the glass products) to completely release the glass stress.
When the stress on the surface of the glass is almost released, the temperature is slowly lowered. Similar to preheating, a slower cooling speed can be used to allow the glass to slowly adapt and avoid explosion due to excessive temperature difference. Usually, it is adjusted to slow cooling between 20° and 30° lower than the annealing temperature.
Finally, the cooling stage is entered. After slow cooling, the cooling speed can be accelerated to shorten the annealing time and save resources. Help the temperature of the glass products to drop to room temperature, so that the performance of the glass can be kept stable, and the glass products will be more transparent, beautiful, durable and strong.
Of course, during the annealing process, we must also pay attention to safety issues like processing glass, and strictly follow the use of glass annealing furnaces; wear protective equipment to avoid glass explosions, high temperature burns and other problems; finally, regularly check circuit equipment and machine parts and equipment to avoid accidents.
How about it, through this simple introduction, do you have an understanding of the process of glass annealing in the furnace? If you are interested in annealing furnaces, welcome to visit our website and consult!